American Elements Terbium Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Terbium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range. Nano Terbium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for terbium nanocrystals has focused on use as a dopant in glass and optical fibers, in phosphors, nanophosphors and doped phosphorous nanoparticles i n nanosensors and nanodevices using caged atoms in nanoparticles doped with a few atoms of terbium as the emitter of green light and for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.
Physical Properties Metric English Comments
Density 8.219 g/cc
0.2969 lb/in³
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
Molecular Weight 158.93 g/mol
158.93 g/mol
Thermal Properties Metric English Comments
Melting Point 1356 °C
2473 °F
Boiling Point 3230 °C
5850 °F
Descriptive Properties Value Comments
Appearance Black
Stability Extremely reactive in air