Material Notes:
General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 10 – 80 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 5 -10 m 2 /g. Nano Tin Oxide Particles are also available in rutile, ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Tin Oxide Nanocrystals include in magnetic resonance, as Magnetic Nanoparticles, and for magnetic data storage and magnetic resonance imaging (MRI) and for its optical properties.
Physical Properties Metric English Comments
Density 6.90 g/cc
0.249 lb/in³
Particle Size 0.020 - 0.040 µm
0.020 - 0.040 µm
0.10 µm
0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
10 - 80 m²/g
10 - 80 m²/g
Molecular Weight 150.69 g/mol
150.69 g/mol
Thermal Properties Metric English Comments
Melting Point 1927 °C
3501 °F
Boiling Point 1900 °C
3450 °F
Descriptive Properties Value Comments
Appearance Black