Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Elements Tungsten Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Tungsten Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 10 – 80 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 5 -10 m 2 /g. Nano Tungsten Oxide Particles are also available in rutile, ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Tungsten Oxide Nanocrystals include in conducting and semi-conducting uses, and for its mechanochemical and optical properties. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.040 µm
0.020 - 0.040 µm
0.10 µm
0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
10 - 80 m²/g
10 - 80 m²/g
Molecular Weight 231.85 g/mol
231.85 g/mol
Descriptive Properties Value Comments
Appearance Black
Users viewing this material also viewed the following: