General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 75 - 100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Yttrium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for yttrium nanocrystals has focused on their potential electrical, magnetic, optical, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.
Physical Properties Metric English Comments
Density 4.472 g/cc
0.1616 lb/in³
Particle Size 0.0050 - 0.045 µm
0.0050 - 0.045 µm
0.075 - 0.10 µm
0.075 - 0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 88.91 g/mol
88.91 g/mol
Thermal Properties Metric English Comments
Melting Point 1526 °C
2779 °F
Boiling Point 3336 °C
6037 °F
Descriptive Properties Value Comments
Appearance Black
Stability Fairly stable in air