American Elements Zirconium Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Zirconium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with specific surface area (SSA) in the 30 – 80 m 2 /g range and also available in with an average particle size of 50 -100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Zirconium Particles are also available in passivated and in Ultra high purity and high purity and carbon coated and dispersed forms. Applications for zirconium nanocrystals include nano-crystalline Zirconium alloys for space applications as alternatives for titanium in components of liquid rocket engines (e.g. lines and turbopumps), since they are lighter and less susceptible to embrittlement by hydrogen, and in nanowire, nanofiber and in certain other alloy and catalyst applications.
Physical Properties Metric English Comments
Density 6.506 g/cc
0.2350 lb/in³
Particle Size 0.010 - 0.040 µm
0.010 - 0.040 µm
0.050 - 0.10 µm
0.050 - 0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
30 - 80 m²/g
30 - 80 m²/g
Molecular Weight 91.22 g/mol
91.22 g/mol
Thermal Properties Metric English Comments
Melting Point 1852 °C
3366 °F
Boiling Point 3580 °C
6480 °F
Descriptive Properties Value Comments
Appearance Black