American Polymers API 410 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer American Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers API 410 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact is needed. Other applications include caps, closures and frames.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 1.97 GPa
285 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °C
189 °F
Annealed; ASTM D648
Vicat Softening Point 97.8 °C
208 °F
ASTM D1525