Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Americas Styrenics LLC
Trade Name STYRON A-TECH®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPackaging for foods such as yot, sour cream, delicatessen salads and gravyContainers and lidsCold temperature packagingPortion dairy containersInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D638
Tensile Strength 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 1.31 GPa
190 ksi
ASTM D638
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 83.9 °C
183 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
ASTM D648
Vicat Softening Point 104 °C
220 °F
ASTM D1525