Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium flow Applications:Pump partsGas meter parts Carriers for grinding wheels , etc. Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.750 - 0.850 g/cc
0.0271 - 0.0307 lb/in³
IS 867-1963
Water Absorption 0.10 - 0.15 %
0.10 - 0.15 %
IS 13411-1993
Linear Mold Shrinkage 0.0020 - 0.0035 cm/cm
0.0020 - 0.0035 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 - 56.0 MPa
6670 - 8120 psi
5 mm/min.; IS 867-1963
Shear Strength 60.0 - 65.0 MPa
8700 - 9430 psi
IS 867-1963
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
IS 13411-1992
Processing Properties Metric English Comments
Mold Temperature 160 - 170 °C
320 - 338 °F
Injection Pressure 15.68 - 34.3 MPa
2274 - 4970 psi
Mold Pressure
Cure Time 1.00 - 1.17 min
0.0167 - 0.0194 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C
Users viewing this material also viewed the following: