Anderman Ceramics EAZ 20 Zirconia Toughened Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Anderman Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Anderman Ceramics EAZ 20 Zirconia Toughened Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.
Physical Properties Metric English Comments
Density 4.30 g/cc
0.155 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 16
16
Tensile Strength 290 MPa
42000 psi
Flexural Strength 448 MPa
65000 psi
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C
4.61 µin/in-°F
Thermal Conductivity 27.0 W/m-K

@Temperature 20.0 - 100 °C
187 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Component Elements Properties Metric English Comments
Al2O3 77 %
77 %
ZrO2 23 %
23 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm

@Temperature 600 °C
1.00e+9 ohm-cm

@Temperature 1110 °F
1.00e+14 ohm-cm

@Temperature 20.0 °C
1.00e+14 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 10.6

@Frequency 1.00e+6 Hz
10.6

@Frequency 1.00e+6 Hz