Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer AorTech Biomaterials
Trade Name Elast-Eon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc. Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Physical Properties Metric English Comments
Molecular Weight >= 95000 g/mol
>= 95000 g/mol
Mn by GPC using polystyrene stds; TM-005
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 70
55 - 70
TM-025
Tensile Strength at Break 25.0 - 35.0 MPa
3630 - 5080 psi
TM-019G
Tensile Stress 13.0 - 17.0 MPa

@Strain 100 %
1890 - 2470 psi

@Strain 100 %
TM-019G
18.0 MPa

@Strain 200 %
2610 psi

@Strain 200 %
23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
Elongation at Break >= 300 %
>= 300 %
TM-019G
Modulus of Elasticity >= 0.200 GPa
>= 29.0 ksi
TM-019E
Tear Strength 129 kN/m
736 pli
Descriptive Properties Value Comments
Polydispersity 1.8-2.4
TM-005; Mw/Mn by GPC using polystyrene stds