Material Notes:
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
Tensile Strength at Break 34.0 MPa
4930 psi
Elongation at Break >= 200 %
>= 200 %
Modulus of Elasticity 0.650 GPa
94.3 ksi