Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Tensile Strength at Break 12.0 MPa
1740 psi
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
5.00 MPa

@Strain 200 %
725 psi

@Strain 200 %
6.00 MPa

@Strain 300 %
870 psi

@Strain 300 %
Elongation at Break >= 700 %
>= 700 %
Modulus of Elasticity 0.0110 GPa
1.60 ksi
Tear Strength 45.0 kN/m
257 pli