Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Composites 8007 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8007 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Pigmentable, Low Water Absorption, Weathering Resistant, Good Corrosion Resistance in Waste Water EnvironmentInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.00090 cm/cm
0.00090 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Hardness, Rockwell M 106
106
ASTM D785
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Tensile Modulus 13.1 GPa
1900 ksi
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
Tangent; ASTM D790
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.70
0.70
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648
Users viewing this material also viewed the following: