Applied Composites 8012 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8012 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: SpecialtyProduct Application: Food EquipmentDistinct Features: NSF ApprovedInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.2 MPa
8000 psi
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
Tangent; ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256