Material Notes:
Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional StabilityInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Tensile Strength, Ultimate 82.7 MPa
12000 psi
ASTM D638
Tensile Modulus 10.3 GPa
1500 ksi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
Secant at 2.5 Deflection; ASTM D790
4.83 GPa
700 ksi
Secant at 0.5 Deflection; ASTM D790
8.96 GPa
1300 ksi
Tangent; ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
Flexural Load; ASTM D648