Material Notes:
Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventional tools, no firing required.
Physical Properties Metric English Comments
Specific Gravity 2.30 g/cc
2.30 g/cc
Porosity 2.3 %
2.3 %
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0
6.0
Flexural Strength 68.9 MPa
10000 psi
Compressive Strength 172 MPa
25000 psi
Thermal Properties Metric English Comments
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.30 W/m-K
9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1150 °C
2100 °F
Electrical Properties Metric English Comments
Dielectric Constant 5.3

@Frequency 1e+6 Hz
5.3

@Frequency 1e+6 Hz
Dielectric Strength 3.94 kV/mm
100 kV/in
Dissipation Factor 0.053

@Frequency 1e+6 Hz
0.053

@Frequency 1e+6 Hz