Material Notes:
Hot-pressed high purity 99% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; bars from 1/4" x 1/4" to 2"x 2".
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
Porosity 22 %
22 %
Mechanical Properties Metric English Comments
Flexural Strength 19.3 MPa
2800 psi
Compressive Strength 33.1 MPa
4800 psi
Thermal Properties Metric English Comments
CTE, linear 0.360 µm/m-°C

@Temperature 20.0 °C
0.200 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 22.00 W/m-K
152.7 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 3000 °C
5430 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
Dielectric Strength 34.1 kV/mm
865 kV/in
Dissipation Factor <= 0.00020

@Frequency 1e+6 Hz
<= 0.00020

@Frequency 1e+6 Hz