Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic

Category Ceramic , Glass , Glass Ceramic , Machinable Ceramic
Manufacturer Aremco
Trade Name AREMCOLOX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High dielectric and mechanical strength. For high voltage insulators, coil forms, soldering fixtures, arc barriers. Readily machined, no firing required. Plates from 1/8" to 1" thick; rods from 1/4" to 1" diameter.
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 5.5
5.5
Flexural Strength 89.6 MPa
13000 psi
Compressive Strength 310 MPa
45000 psi
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 20.0 °C
6.00 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.867 W/m-K
6.02 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 399 °C
750 °F
Electrical Properties Metric English Comments
Dielectric Constant 6.7

@Frequency 1e+6 Hz
6.7

@Frequency 1e+6 Hz
Dielectric Strength 28.7 kV/mm
730 kV/in
Dissipation Factor 0.0090

@Frequency 1e+6 Hz
0.0090

@Frequency 1e+6 Hz
Users viewing this material also viewed the following: