Material Notes:
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and coefficient of thermal expansion similar to most metals and sealing glasses. Machines to tight tolerances up to 0.0005”, surface finish of less than 20µin, and polishes to a smoothness of 0.5µin. Used for ultra high vacuum, aerospace, nuclear, wielding, fixturing, and medical applications. Readily machined and no firing required. Bars, disks, rods and plates are available fro 1/16” thick up to 12” diameter.
Physical Properties Metric English Comments
Specific Gravity 2.52 g/cc
2.52 g/cc
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 93.8 MPa
13600 psi
Compressive Strength 345 MPa
50000 psi
Thermal Properties Metric English Comments
CTE, linear 12.6 µm/m-°C

@Temperature 20.0 °C
7.00 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.46 W/m-K
10.2 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 800 °C
1470 °F
Electrical Properties Metric English Comments
Dielectric Constant 6.0

@Frequency 1e+6 Hz
6.0

@Frequency 1e+6 Hz
Dielectric Strength 30.9 kV/mm
785 kV/in
Dissipation Factor 0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz