Material Notes:
Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity 35000 cP
35000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Shear Strength 33.09 MPa
4800 psi
ASTM D1002-94
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C
33.0 µin/in-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Shrinkage 0.00100 %
0.00100 %
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Strength 43.3 kV/mm
1100 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
alternate cure
1440 - 2880 min

@Temperature 79.4 °C
24.0 - 48.0 hour

@Temperature 175 °F
recommended cure
Pot Life 60.0 min

@Temperature 25.0 °C
60.0 min

@Temperature 77.0 °F
100 gm mass
Descriptive Properties Value Comments
Chemical Resistance Good
Color Off-White
Mix Ratio 2:1