Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Aremco-Bond™ 657 High Performance Epoxide

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Aremco
Trade Name Aremco-Bond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Bond™ 657 High Performance Epoxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stainless Steel-Filled, High Corrosion Resistance.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Shear Strength 17.2 MPa
2500 psi
ASTM D1002-94
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Shrinkage 0.20 %
0.20 %
Cure Shrinkage
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
Recommended Cure
1440 - 2880 min

@Temperature 23.0 °C
24.0 - 48.0 hour

@Temperature 73.4 °F
Alternate
Pot Life 4.20 min

@Temperature 25.0 °C
4.20 min

@Temperature 77.0 °F
100 gm mass
Descriptive Properties Value Comments
Chemical Resistance Excellent
Mix Ratio By Weight 1:1
resin:hardener
Users viewing this material also viewed the following: