Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Epoxy , Epoxy, High Temperature
Manufacturer Aremco
Trade Name Corr-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag houses, cyclones, hoppers and other process equipment used in the power, pulp and paper, and chemical processing industries.
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
Solids Content 100 %
100 %
weight
100 %
100 %
volume
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Thickness >= 1270 microns
>= 50.0 mil
estimated wet film thickness
>= 1270 microns
>= 50.0 mil
recommended dry film thickness
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
for Epoxy Coating
Elongation at Break 2.0 %
2.0 %
for Epoxy Coating
Flexural Strength 79.3 MPa
11500 psi
for Epoxy Coating
Compressive Strength 82.7 MPa
12000 psi
for Epoxy Coating
Adhesive Bond Strength 6.21 MPa

@Temperature 175 °C
900 psi

@Temperature 347 °F
Lap Shear Strength vs. Aluminum
8.27 MPa

@Temperature 150 °C
1200 psi

@Temperature 302 °F
Lap Shear Strength vs. Aluminum
13.8 MPa

@Temperature 100 °C
2000 psi

@Temperature 212 °F
Lap Shear Strength vs. Aluminum
15.9 MPa

@Temperature 25.0 °C
2300 psi

@Temperature 77.0 °F
Lap Shear Strength vs. Aluminum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Flash Point >= 93.3 °C
>= 200 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Dry Time 4.00 hour
4.00 hour
Touch
4.00 - 8.00 hour
4.00 - 8.00 hour
Recoat
6.00 - 8.00 hour
6.00 - 8.00 hour
Handling
Cure Time 360 min

@Temperature 121 °C
6.00 hour

@Temperature 250 °F
>8 Hour Air Set Required Prior to Curing
2880 min

@Temperature 22.2 °C
48.0 hour

@Temperature 72.0 °F
>8 Hour Air Set Required Prior to Curing
Pot Life 45.0 min

@Temperature 23.0 °C
45.0 min

@Temperature 73.4 °F
Shelf Life 12.0 Month

@Temperature 23.0 °C
12.0 Month

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Gray
Dry Film Coverage ft2/gal 1604
at 1 mil
Mix Ratio By Weight 100:8
Novolac:Epoxy
Mixed Viscosity Paste
Primer Not Required or Recommended
Thinner Not Required or Recommended