Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%

Category Ceramic , Oxide
Manufacturer Aremco
Trade Name Pyro-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their alloys. Usable in vacuum and inert atmospheres to 3630 °F (2000 °C).
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
Solids Content 23 %
23 %
volume
42.7 %
42.7 %
weight
pH 7.0 - 8.0
7.0 - 8.0
Coating pH
Viscosity 200 - 400 cP
200 - 400 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1500 °C
2732 °F
Flash Point 23.9 °C
75.0 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 60.0 min

@Temperature 93.3 °C
1.00 hour

@Temperature 200 °F
>0.5 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Off-White
Coverage ft2/gal 370
Theoretical Coverage at 1 mil dry film thickness
Thinner 634-YO-T
Weight/Gallon 12 lbs