Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Pyro-Tape™ 682-PM High Temperature Tape Tri-layer silicone rubber/aluminum foil/ fiberglass with silicone adhesive

Category Polymer , Adhesive , Tape
Manufacturer Aremco
Trade Name Pyro-Tape™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Tape™ 682-PM High Temperature Tape Tri-layer silicone rubber/aluminum foil/ fiberglass with silicone adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications Plasma Spray Masking Features Multi-ply construction replaces single-ply tapes permitting significant reduction in masking time. Shadow mask tape for HVOF (high velocity oxy- fuel) spraying.
Physical Properties Metric English Comments
Thickness 483 microns
19.0 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -73.0 °C
-99.4 °F
Descriptive Properties Value Comments
Adhesion 40 oz/in
Tape Tensile Strength 130 lbs/in