Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group EVATANE® 28-800 Copolymer Ethylene - Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Arkema
Trade Name Evatane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group EVATANE® 28-800 Copolymer Ethylene - Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVATANE® 28-800 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-800 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 28-800 brings softness, flexibility and polarity. EVATANE® 28-800 is compatible with tackifying resins and waxes. It’s a useful product for hot melt adhesives formulation. EVATANE® 28-800 delivers high cohesive strength with any kind of fillers (masterbatchs). It can also be used as an additive for crude oil (pour point depressant)Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.950 g/cc

@Temperature 23.0 °C
0.0343 lb/in³

@Temperature 73.4 °F
ISO 1183
Vinyl Acetate Content 27 - 29 %
27 - 29 %
FTIR (internal)
Melt Index of Compound 700 - 900 g/10 min

@Load 2.16 kg,
Temperature 190 °C
700 - 900 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength at Break 1.50 MPa
218 psi
ASTM D638
Elongation at Break 300 - 500 %
300 - 500 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 61.0 °C
142 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 0.999 kg
<= 104 °F

@Load 2.20 lb
ISO 306
Ring & Ball Softening Point 76.0 °C
169 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F