Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermomechanical properties.Main applications of Kynar FLEX: corrosion protection in the chemical industry, coating (painting, coextrusion), off shore, wire and cable.Kynar FLEX 2750 is a grade of granules to be used where maximum flexibility or impact strength is required.Powder form available as Kynar FLEX 2751.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Melt Flow 1.9 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.9 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 16 %
16 %
50 mm/min
Tensile Modulus 0.480 GPa
69.6 ksi
1 mm/min
Charpy Impact, Notched 11.8 J/cm²
56.2 ft-lb/in²
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Melting Point 135 °C
275 °F
10°C/min
Vicat Softening Point 61.0 °C
142 °F
50°C/hr; 50N
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
10°C/min
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Oxygen Index 49 %
49 %
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 7.1

@Frequency 1e+6 Hz
7.1

@Frequency 1e+6 Hz
11.4

@Frequency 100 Hz
11.4

@Frequency 100 Hz
Dissipation Factor 0.024

@Frequency 100 Hz
0.024

@Frequency 100 Hz
Copyright © lookpolymers.com All Rights Reserved