Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

Category Polymer , Thermoplastic , EMAAA Terpolymer
Manufacturer Arkema
Trade Name LOTADER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lamination, designed as: Concentrate to be used in dry blend with LDPE. LOTADER 4210 improves adhesion of LDPE on aluminum foils, metallized or primerized films.Ready for use resin to be used pure.LOTADER 4210 gives excellent adhesion on substrates like alu foil, metallized plastics, paper, board, PE and some plastic films.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Butyl Acrylate Content 6.5 %
6.5 %
IRTF (internal)
Melt Index of Compound 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
DSC
Vicat Softening Point 69.0 °C

@Load 0.999 kg
156 °F

@Load 2.20 lb
ASTM D1525
Brittleness Temperature <= -50.0 °C
<= -58.0 °F
ASTM D726
Processing Properties Metric English Comments
Processing Temperature 270 - 330 °C
518 - 626 °F
Descriptive Properties Value Comments
Maleic Anhydride Content (%) 3.6
IRTF (internal)