Material Notes:
LOTADER AX 8840 is a random copolymer of Ethylene and Glycidyl Methacrylate, polymerized under high pressure in an autoclave process. Due to the reactivity induced by the Glycidyl methacrylate, LOTADER AX 8840 can be use as a compatibilizer for Polyesters/Polyolefins blends and as an adhesive for some laminate structures (Polyolefins/Polyesters, Polyolefins/PPS etc.).Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Modulus of Elasticity 0.104 GPa
15.1 ksi
ASTM D638
Flexural Modulus 0.0850 GPa
12.3 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
DSC
Vicat Softening Point 87.0 °C

@Load 0.999 kg
189 °F

@Load 2.20 lb
ASTM D1525
Descriptive Properties Value Comments
Glycidyl Methacrylate Content (%) 8
IRTF (internal)