Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Extrusion Grade
Manufacturer Arkema
Trade Name LOTRYL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of choice for applications where softness, flexibility and polarity are required. Typical applications are extrusion-coating, coextrusion and compounds.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.960 g/cc

@Temperature 23.0 °C
0.0347 lb/in³

@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 17 - 20 %
17 - 20 %
IRTF (internal)
Melt Index of Compound 2.0 - 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 - 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 25
25
ASTM D2240
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.0500 GPa
7.25 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
DSC
Vicat Softening Point 53.0 °C

@Load 1.02 kg
127 °F

@Load 2.25 lb
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F