Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer Arkema
Trade Name LOTRYL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polymer of choice for applications where softness, flexibility and polarity are required.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 19 - 22 %
19 - 22 %
IRTF (internal)
Melt Index of Compound 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Modulus 0.0200 GPa
2.90 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 80.0 °C
176 °F
DSC
Vicat Softening Point 46.0 °C

@Load 1.02 kg
115 °F

@Load 2.25 lb
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Users viewing this material also viewed the following: