Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer Arkema
Trade Name LOTRYL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polymer of choice for applications where softness, flexibility and polarity are required.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.950 g/cc

@Temperature 23.0 °C
0.0343 lb/in³

@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 27 - 31 %
27 - 31 %
IRTF (internal)
Melt Index of Compound 2.0 - 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 - 3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.00800 GPa
1.16 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 61.0 °C
142 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 1.02 kg
<= 104 °F

@Load 2.25 lb
ASTM D1525
Ring & Ball Softening Point 175 °C
347 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F