Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Arkema
Trade Name LOTRYL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formulations and in film applications.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.930 g/cc

@Temperature 23.0 °C
0.0336 lb/in³

@Temperature 73.4 °F
ISO 1183
Butyl Acrylate Content 27 - 32 %
27 - 32 %
IRTF (internal)
Melt Index of Compound 1.5 - 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 - 2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D638
Elongation at Break 850 %
850 %
ASTM D638
Flexural Modulus 0.00900 GPa
1.31 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 78.0 °C
172 °F
DSC
Vicat Softening Point 41.0 °C

@Load 1.02 kg
106 °F

@Load 2.25 lb
ASTM D1525
Ring & Ball Softening Point >= 190 °C
>= 374 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Users viewing this material also viewed the following: