Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Arkema
Trade Name Nakan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NAKAN RPS 400 M is a rigid polyvinyl chloride compound developed for extrusion of cables ducts.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.8 %
5.8 %
50 mm/min
Tensile Modulus 3.02 GPa
438 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 80.5 °C
177 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in