Material Notes:
NAKAN RRS 401 L is a rigid polyvinyl chloride compound developed for injection molding of waste water fittings.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
50 mm/min
Elongation at Break 25 %
25 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
Vicat Softening Point 73.0 °C
163 °F
50°C/hr; 50N
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 46 %
46 %