Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group OREVAC® 18707 Grafted Maleic Anhydride Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Arkema
Trade Name OREVAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 18707 Grafted Maleic Anhydride Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC 18707 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18707 is an extrusion adhesive to be used in coextrusion technologies. As adhesive, OREVAC 18707 has been designed to develop adhesion between PP and EVOH or PP and PA .Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Index of Compound 4.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 620 %
620 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 152 °C
306 °F
DSC
Vicat Softening Point 123 °C
253 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 230 °C
446 °F
Adapter Temperature 230 °C
446 °F
Die Temperature 230 °C
446 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved