Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P are mainly used in application where mechanical and adhesive performances at high temperatures are required. These Orevac are used as tie layer in 3 layer polypropylene coatings (epoxy primer / adhesive / polypropylene) for external protection of steel pipe.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ISO 1183
Particle Size <= 125 µm
<= 125 µm
0.2
100 - 300 µm
100 - 300 µm
0.65
300 - 400 µm
300 - 400 µm
0.15
>= 400 µm
>= 400 µm
0
Melt Index of Compound 6.0 - 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 6.0
6.0
ISO 608
Tensile Strength at Break 20.0 MPa
2900 psi
ISO R 527-2
Elongation at Break 500 %
500 %
ISO R 527-2
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
DSC
Vicat Softening Point 120 °C

@Load 0.999 kg
248 °F

@Load 2.20 lb
ISO 306