Arkema Group OREVAC® 9304 EVA Terpolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 9304 EVA Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include blown film extrusions, thermo-adhesive films, and hot melt adhesives.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Vinyl Acetate Content 23.5 - 26.5 %
23.5 - 26.5 %
Arkema
Melt Index of Compound 5.5 - 9.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 - 9.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
26.0 MPa
3770 psi
Film Property, 50 µm thickness; ASTM D882
Tensile Strength, Yield 2.60 MPa
377 psi
ASTM D638
4.00 MPa
580 psi
Film Property, 50 µm thickness; ASTM D882
Elongation at Break 600 - 900 %
600 - 900 %
ASTM D638
700 - 900 %
700 - 900 %
Film Property, 50 µm thickness; ASTM D882
Dart Drop Test 400 g
0.882 lb
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 80.0 °C
176 °F
DSC
Vicat Softening Point 49.0 °C
120 °F
ASTM D1525
Ring & Ball Softening Point 153 °C
307 °F
Optical Properties Metric English Comments
Haze 4.6 %
4.6 %
50 micron film; ASTM D1003
Descriptive Properties Value Comments
MAH Mini 1600