Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA Terpolymers based Main Application: Cast film coextrusionInformation provided by Arkema Group
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Vinyl Acetate Content 8.0 - 9.5 %
8.0 - 9.5 %
Melt Flow 3.3 - 4.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.3 - 4.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38.6
38.6
ISO 868
Tensile Strength at Break 20.6 MPa
2990 psi
50 microns film; ASTM D882
Tensile Strength, Yield 6.50 MPa
943 psi
50 microns film; ASTM D882
Elongation at Break 555 %
555 %
50 microns film; ASTM D882
Modulus of Elasticity 0.0695 GPa
10.1 ksi
ISO R527
Dart Drop Test 355 g
0.783 lb
50 microns film
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
D.S.C. method
Vicat Softening Point 77.0 °C
171 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 7.6 %
7.6 %
50 micron film; ASTM D1003