Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned)

Category Polymer , Thermoplastic , Nylon
Manufacturer Arkema
Trade Name Orgalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISO data provided by the manufacturer, Arkema.
Mechanical Properties Metric English Comments
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.700 GPa
102 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Melting Point 220 °C
428 °F
10°C/min
Oxygen Index 30 %
30 %
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V