Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness, nice touch feeling) Matrix for volatile substances (perfumes) IndustrialISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 235 °C
14 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 25
25
Tensile Strength, Yield 2.80 MPa

@Strain 50.0 %
406 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.0100 GPa
1.45 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
NB
NB
Low Temp
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Melting Point 134 °C
273 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 42.0 °C
108 °F
Vicat Softening Point 60.0 °C
140 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+12 ohm
3.00e+12 ohm