Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion SportISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Melt Flow 5.0 g/10 min

@Load 1.00 kg,
Temperature 235 °C
5.0 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.54 J/cm²
7.33 ft-lb/in²
0.780 J/cm²

@Temperature -30.0 °C
3.71 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 176 °C
349 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Vicat Softening Point 165 °C
329 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.