Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion SportISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Water Absorption 0.90 %
0.90 %
Moisture Absorption at Equilibrium 0.70 %
0.70 %
Humidity Absorption
Melt Flow 5.0 g/10 min

@Load 1.00 kg,
Temperature 235 °C
5.0 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
Thermal Properties Metric English Comments
Melting Point 176 °C
349 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity 7.74e+13 ohm-cm
7.74e+13 ohm-cm
Surface Resistance 1.84e+14 ohm
1.84e+14 ohm
Dielectric Strength 44.5 kV/mm
1130 kV/in
Dissipation Factor 0.00037

@Frequency 1e+6 Hz
0.00037

@Frequency 1e+6 Hz
0.00074

@Frequency 100 Hz
0.00074

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V