Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MP 1878 SA 01 Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MP 1878 SA 01 Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyether block amide PEBAX® MP 1878 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. Added to PA6 Pebax® MP 1878 enhances the properties of PA6, especially at low temperatures and low humidity content, at the same time maintaining the transparency of the nylon film and improving its soft touch. This SA grade is specially designed to medical and food uses.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 6.7 %

@Temperature 23.0 °C,
Time 86400 sec
6.7 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.35 %

@Temperature 20.0 °C
1.35 %

@Temperature 68.0 °F
50% RH; ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
54

@Time 15.0 sec
54

@Time 0.00417 hour
Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 60.0 MPa
8700 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break 550 %
550 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.180 GPa
26.1 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Thermal Properties Metric English Comments
Melting Point 195 °C
383 °F
ISO 11357
Vicat Softening Point 169 °C

@Load 1.02 kg
336 °F

@Load 2.25 lb
ISO 306
Users viewing this material also viewed the following: