Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Melt Flow 7.3 g/10 min

@Load 1.00 kg,
Temperature 235 °C
7.3 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 15.0 MPa
2180 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 28 %
28 %
50 mm/min
Tensile Modulus 0.227 GPa
32.9 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
(Dry)
Vicat Softening Point 155 °C
311 °F
50°C/hr; 50N
Oxygen Index 22.9 %
22.9 %
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Surface Resistance 5.00e+11 ohm
5.00e+11 ohm
Users viewing this material also viewed the following: