Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness, nice touch feeling...) Industrial (damping properties, overmolding, resiliency...)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Water Absorption 1.5 %
1.5 %
Moisture Absorption at Equilibrium 0.40 %
0.40 %
Humidity Absorption
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 235 °C
14 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Tensile Strength, Yield 6.90 MPa

@Strain 50.0 %
1000 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.0650 GPa
9.43 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 147 °C
297 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity 1.57e+13 ohm-cm
1.57e+13 ohm-cm
Surface Resistance 6.98e+12 ohm
6.98e+12 ohm
Dielectric Strength 43.0 kV/mm
1090 kV/in
Dissipation Factor 0.00059

@Frequency 1e+6 Hz
0.00059

@Frequency 1e+6 Hz
0.00085

@Frequency 100 Hz
0.00085

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V