Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 20% Glass Fiber Filled
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined with good impact strength. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.Example applications: Mechanical fittings.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 12.9 g/10 min

@Load 2.16 kg,
Temperature 235 °C
12.9 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.0 MPa
10400 psi
5 mm/min
Elongation at Break 8.0 %
8.0 %
5 mm/min
Tensile Modulus 3.83 GPa
556 ksi
1 mm/min
Charpy Impact Unnotched 6.40 J/cm²
30.5 ft-lb/in²
6.87 J/cm²

@Temperature -30.0 °C
32.7 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
0.720 J/cm²

@Temperature -30.0 °C
3.43 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point 151 °C
304 °F
50°C/hr; 50N