Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.Example applications: Mechanical parts with very high rigidity.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
Melt Flow 1.1 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 150 MPa
21800 psi
5 mm/min
Elongation at Break 4.0 %
4.0 %
5 mm/min
Tensile Modulus 15.9 GPa
2310 ksi
1 mm/min
Charpy Impact Unnotched 8.95 J/cm²
42.6 ft-lb/in²
8.75 J/cm²

@Temperature -30.0 °C
41.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 2.32 J/cm²
11.0 ft-lb/in²
1.76 J/cm²

@Temperature -30.0 °C
8.38 ft-lb/in²

@Temperature -22.0 °F