Arkema Group Rilsan® Powder D40 Natural Nylon 11, Coating Grade

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Powder
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® Powder D40 Natural Nylon 11, Coating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture depending on the granulometry used. Can be dispersed completely in liquid media.Excellent chemical resistance.The range includes several colors.The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.9 %
1.9 %
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
10°C/min
Vicat Softening Point 160 °C
320 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in