Material Notes:
Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDERMelt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.There is a wide range of colors.The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Water Absorption 1.9 %
1.9 %
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
10°C/min
Vicat Softening Point 160 °C
320 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in