Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Elastomer, for Thermal Management
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.008 in., +0.000,-0.002(0.2 mm, +0.00, -0.05) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in +0.000,-0.002(0.2 mm, +0.00, -0.05). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: White. Weight: 525.5 g/m² ± 50.9 (15.5 oz./yd.² ± 1.5). Shelf Life: 3 months from date of manufacture at 4.4°C ± 2.8°C (40°F ±5°F). Maximum Thermal Impendence is 0.2°C/W.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Shear Modulus 0.000350 - 0.000450 GPa
0.0508 - 0.0653 ksi
Adhesive Bond Strength >= 1.40 MPa
>= 203 psi
lap shear strength
Thermal Properties Metric English Comments
Thermal Conductivity >= 1.20 W/m-K
>= 8.33 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.6 °C
-69.9 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.75 kV/mm
400.0 kV/in
Processing Properties Metric English Comments
Processing Temperature 138 °C
280 °F
curing temp.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved